Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.050 cm/cm | 0.050 in/in | ASTM D955 |
Multibase Multi-Pro® 4012 X Platinum Polypropylene Glass Fiber Reinforced, 42% by weight.Forms:PelletsProcessing Methods:Injection MoldingFeatures:Appearance, Pleasing SurfaceUses:AppliancesInformation provided by Multibase |
|||
Linear Mold Shrinkage | <= 0.050 cm/cm @Temperature 70.0 °C, Time 605000 sec |
<= 0.050 in/in @Temperature 158 °F, Time 168 hour |
|
Monmouth Rubber & Plastics Durafoamâ„¢ S88 PVC/NBR Information provided by Monmouth Rubber & Plastics Corp. |
|||
Linear Mold Shrinkage | 0.050 - 0.060 cm/cm | 0.050 - 0.060 in/in | ASTM D955 |
Lubrizol Isoplast® 300 Engineering Thermoplastic Polyurethane Resin Type: Isoplast® 300 is an engineering thermoplastic polyurethane resin.Appearance: Clear transparent pelletsApplication: Sheet extrusion, composite structures for industrial and consumer goods, inj.. |
|||
Linear Mold Shrinkage | 0.050 cm/cm @Thickness 80.0 mm |
0.050 in/in @Thickness 3.15 in |
sheet; ASTM D4894 |
3M Dyneon™ TFM™ 4220 Modified PTFE, 2% Cond. Pigm. Filled
(discontinued **) Applications include antistat linings, seals, gaskets, moldings.Data provided by Dyneon. |