Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.0450 cm/cm | 0.00200 - 0.0450 in/in | Average value: 0.00606 cm/cm Grade Count:250 |
Overview of materials for Polystyrene, Impact Modified This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Impact Modified". Each property range of values reported is minimum and maximum values of a.. |
|||
Linear Mold Shrinkage | 0.0200 - 0.0450 cm/cm | 0.0200 - 0.0450 in/in | Average value: 0.0272 cm/cm Grade Count:12 |
Overview of materials for Polytetrafluoroethylene (PTFE), Conductive Carbon Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Conductive Carbon Filled". Each property range of values reported is min.. |
|||
Linear Mold Shrinkage | 0.00500 - 0.0450 cm/cm | 0.00500 - 0.0450 in/in | Average value: 0.0123 cm/cm Grade Count:15 |
Overview of materials for Thermoplastic Polyurethane (TPUR), Polyether Grade This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyurethane (TPUR), Polyether Grade". Each property range of values reported is minimum a.. |