Polymer Property : Linear Mold Shrinkage = 0.0305 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0305 cm/cm
0.0305 in/in
1/8" Bar
BASF Ultramid® 8202 L Intermediate PA6 (Conditioned)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..
Linear Mold Shrinkage 0.0305 cm/cm
0.0305 in/in
1/8" Bar
BASF Ultramid® 8202 L Intermediate PA6 (Dry)
Description: Ultramid 8202 L-Intermediate is an unreinforced, low viscosity, non-lubricated PA6 injection molding homopolymer exhibiting excellent melt fluidity for filling thin sections. It is avai..