Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0234 cm/cm

@Thickness 4.00 mm
0.0234 in/in

@Thickness 0.157 in
Azoty Tarnow™ TARNOFORM 300 XEC1 POM
Electrically conductive, carbon fiber reinforced injection molding grade suitable for the applications where increased strength and stiffness is required.Information provided by Zakłady Azotowe ..