Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0226 cm/cm
0.0226 in/in
Plastcom SLOVALEN PH 59 GB 20 PP, 20% glass beads, mod. of mech. prop.
FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP...