Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0226 cm/cm | 0.0226 in/in | |
Plastcom SLOVALEN PH 59 GB 20 PP, 20% glass beads, mod. of mech. prop. FeaturesModified homopolymer PP for injection moulding, chemically reinforced with 20% glass beads, contains the modifier of mechanical properties. Increased strength in comparison with unfilled PP... |