Polymer Property : Linear Mold Shrinkage = 0.0212 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00600 - 0.0212 cm/cm
0.00600 - 0.0212 in/in
Average value: 0.0113 cm/cm Grade Count:105
Overview of materials for Polypropylene with 30% Talc Filler
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 30% Talc Filler". Specific grades with primary filler content between 25% and 34% are..