Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0189 cm/cm | 0.0189 in/in | |
Plastcom SLOVALEN PH 49 GF 40 PP, 40% glass fibre PP homopolymer for injection moulding, chemically strengthened with 40% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-go.. |