Material Notes:
PP homopolymer for injection moulding, chemically strengthened with 40% of glass fibre, for mouldings with high strength and toughness used in the automotive, electrical, engineering and consumer-goods industry.Delivered in natural mode and in the full RAL colour scale.Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.000 kg palette, in paper octabins with a thick PE foil fixed on a 1.000 kg palette or in other packaging according to customer requirements. The transport is provided in closed-up vehicles where the material is protected against movement and mechanical damage. The product requires stocking in closed-up, dry places protected against sun and thermal radiation.Information Provided by Plastcom spol. s r.o.
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Linear Mold Shrinkage 0.0189 cm/cm
0.0189 in/in
Linear Mold Shrinkage, Transverse 0.0165 cm/cm
0.0165 in/in
Melt Flow 5.0 g/10 min

@Load 0.325 kg,
Temperature 270 °C
5.0 g/10 min

@Load 0.716 lb,
Temperature 518 °F
Mechanical Properties Metric English Comments
Tensile Strength at Break 100 MPa
14500 psi
Elongation at Break 3.0 %
3.0 %
Tensile Modulus 8.00 GPa
1160 ksi
Flexural Strength 130 MPa
18900 psi
Flexural Modulus 6.50 GPa
943 ksi
Charpy Impact Unnotched 4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
4.50 J/cm²

@Temperature -20.0 °C
21.4 ft-lb/in²

@Temperature -4.00 °F
Charpy Impact, Notched 0.800 J/cm²

@Temperature -20.0 °C
3.81 ft-lb/in²

@Temperature -4.00 °F
4.50 J/cm²

@Temperature 23.0 °C
21.4 ft-lb/in²

@Temperature 73.4 °F
Thermal Properties Metric English Comments
Melting Point 160 °C
320 °F
Processing Properties Metric English Comments
Melt Temperature 230 - 260 °C
446 - 500 °F
Mold Temperature 50.0 - 70.0 °C
122 - 158 °F
Drying Temperature 80.0 °C
176 °F
Dry Time 4 hour
4 hour
Moisture Content 0.20 %
0.20 %
Injection Pressure 70.0 - 120 MPa
10200 - 17400 psi