Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0183 cm/cm
0.0183 in/in
Plastcom SLOVALEN PC 71 T 10 PP, 10% mineral filling
FeaturesModified copolymer PP for injection moulding with the content of 10% mineral filling. Increased rigidity, strength and thermal use up to 130°C depending on the talc content. Decr eased shri..
Linear Mold Shrinkage 0.0183 cm/cm
0.0183 in/in
STN 64 0808
Plastcom SLOVALEN PH 51 T 10 Polypropylene Homopolymer, 10% Mineral Filled
FeaturesModified homopolymer PP for injection moulding with the content of 10% mineral filler. Increased rigidity, strength and thermal use up to 120°C. Decreased shrinkage. General application ..