Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0160 cm/cm | 0.0160 in/in | ASTM D955 |
Niche Polymer PA66BK Nylon 66 Information provided by Niche Polymer |
|||
Linear Mold Shrinkage | 0.0160 - 0.0500 cm/cm | 0.0160 - 0.0500 in/in | Average value: 0.0300 cm/cm Grade Count:15 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |