Niche Polymer PA66BK Nylon 66

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Unreinforced
Manufacturer Niche Polymer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Niche Polymer PA66BK Nylon 66.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Niche Polymer
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0160 cm/cm
0.0160 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 68.9 MPa
10000 psi
ASTM D638
Elongation at Break 50.0 %
50.0 %
ASTM D638
Flexural Strength 110 MPa
16000 psi
ASTM D790
Flexural Modulus 2.83 GPa
410 ksi
ASTM D790
Izod Impact, Unnotched 0.534 J/cm

@Thickness 3.17 mm
1.00 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 77.8 °C
172 °F
ASTM D648
Processing Properties Metric English Comments
Melt Temperature 254 - 266 °C
489 - 511 °F
ASTM D789
Descriptive Properties Value Comments
Color Black