Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0140 - 0.0270 cm/cm
0.0140 - 0.0270 in/in
Average value: 0.0195 cm/cm Grade Count:7
Overview of materials for Styrene/Butadiene/Styrene (SBS)
This property data is a summary of similar materials in the MatWeb database for the category "Styrene/Butadiene/Styrene (SBS)". Each property range of values reported is minimum and maximum values o..
Linear Mold Shrinkage 0.0140 cm/cm
0.0140 in/in
Average value: 0.0140 cm/cm Grade Count:5
Overview of materials for Nylon 6, Film Grade
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Film Grade". Each property range of values reported is minimum and maximum values of appropriat..