Polymer Property : Linear Mold Shrinkage = 0.0137 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0137 cm/cm
0.0137 in/in
ASTM D955
RheTech Products UVFT3082-74 Thermoplastic Polyolefin, 135K Flexural Modulus, UV Stabilized, Exterior DX9 Black
Applications: Step padsHitch padsExterior trimInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0137 cm/cm
0.0137 in/in
ASTM D955
Multibase Multi-Flex® TPE A 3104-8
Multi-Flex TPE contains Kratonâ„¢ G.Data provided by Multibase.