Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00200 - 0.00950 cm/cm | 0.00200 - 0.00950 in/in | Average value: 0.00675 cm/cm Grade Count:4 |
Overview of materials for Nylon 66/6, 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66/6, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are incl.. |