Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.0077 cm/cm | 0.0077 in/in | Isotropy |
Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product of.. |