Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Glass Fiber Filled
Manufacturer Solvay
Trade Name Technyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Solvay TECHNYL® A 218HP V35 PA66, 35% glass fiber, DRY.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: TECHNYL® A 218HP V35 is a polyamide 6.6, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product offers an outstanding long term heat resistance and is suitable to work in environments characterized by a very high temperature. Available in: Asia Pacific, Europe and Latin AmericaRegulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.Applications: It is used in a wide variety of industries, especially in automotive industry for air circuit parts such as intercoolers.Information provided by Rhodia, Rhodia has been acquired by Solvay.
Physical Properties Metric English Comments
Density 1.39 g/cc
0.0502 lb/in³
ISO 1183/A
Linear Mold Shrinkage 0.0077 cm/cm
0.0077 in/in
Isotropy
Linear Mold Shrinkage, Flow 0.0046 cm/cm
0.0046 in/in
Linear Mold Shrinkage, Transverse 0.0060 cm/cm
0.0060 in/in
Mechanical Properties Metric English Comments
Tensile Strength at Break 170 MPa
24700 psi
ISO 527 Type 1A
Tensile Stress 35.0 MPa

@Strain 1.00 %,
Temperature 200 °C
5080 psi

@Strain 1.00 %,
Temperature 392 °F
45.0 MPa

@Strain 3.00 %,
Temperature 200 °C
6530 psi

@Strain 3.00 %,
Temperature 392 °F
50.0 MPa

@Strain 4.00 %,
Temperature 200 °C
7250 psi

@Strain 4.00 %,
Temperature 392 °F
100 MPa

@Strain 1.00 %,
Temperature 23.0 °C
14500 psi

@Strain 1.00 %,
Temperature 73.4 °F
180 MPa

@Strain 2.00 %,
Temperature 23.0 °C
26100 psi

@Strain 2.00 %,
Temperature 73.4 °F
400 MPa

@Strain 2.00 %,
Temperature 200 °C
58000 psi

@Strain 2.00 %,
Temperature 392 °F
Elongation at Break 2.8 %
2.8 %
ISO 527 Type 1A
Tensile Modulus 10.7 GPa
1550 ksi
ISO 527 Type 1A
Flexural Strength 250 MPa
36300 psi
ISO 178
Flexural Modulus 8.70 GPa
1260 ksi
ISO 178
Charpy Impact Unnotched 7.50 J/cm²
35.7 ft-lb/in²
ISO 179/1eU
Charpy Impact, Notched 1.30 J/cm²
6.19 ft-lb/in²
ISO 179/1eA
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 247 °C
477 °F
ISO 75/Af
Processing Properties Metric English Comments
Feed Temperature 260 - 270 °C
500 - 518 °F
Front Barrel Temperature 280 - 290 °C
536 - 554 °F
Mold Temperature 70.0 - 100 °C
158 - 212 °F
Drying Temperature 80.0 °C
176 °F
Moisture Content <= 0.12 %
<= 0.12 %
Descriptive Properties Value Comments
Compression Zone 270-280°C