Polymer Property : Linear Mold Shrinkage = 0.0068 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0068 cm/cm
0.0068 in/in
Plastcom SLOVAMID 6 CF 20 PA6, 20% carbon fibre
FeaturesChemically reinforced with 20 % carbon fibre, suitable for mouldings with high strength and toughness also at minus temperatures. Used in the automotive, engineering and electrical industry...
Linear Mold Shrinkage 0.0068 cm/cm
0.0068 in/in
Plastcom SLOVALEN PH 66 GF 30 FRO 4 PP, 30% glass fibre, mod. of mech. prop.
Packaging, transport, stockingThe product is packed in hermetically closed thick-walled 25 kg PE bags, on a 1.000 kg palette coated in a stretch foil, in big bags with a thick PE foil fixed on a 1.0..
Linear Mold Shrinkage 0.0068 cm/cm
0.0068 in/in
STN 64 0808
Plastcom SLOVAMID 6 GF 20 Polyamide 6, 20% Glass Fiber
FeaturesPA 6 for injection moulding, chemically coupled with 20% glass fiber. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and con..
Linear Mold Shrinkage 0.0068 cm/cm
0.0068 in/in
ASTM D955
Plenco 00714 Melamine-Phenolic, Granular, Injection Molded
PLENCO 00714 is a melamine-phenolic copolymer molding compound, offering excellent arc resistance and comparative track index values. Type ASTM D 5948 CMG, and UL recognized under component file E4..
Linear Mold Shrinkage 0.0068 cm/cm
0.0068 in/in
ASTM D955
Plenco 4414 Phenolic, Granular, Injection Molded
PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional ..
Linear Mold Shrinkage 0.0068 cm/cm
0.0068 in/in
Plastcom SLOVAMID 6 NG GF 20 PA6, 20% glass fibre
FeaturesPA 6 for injection moulding, chemically strengthened with 20% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and..