Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0015 - 0.0032 cm/cm
0.0015 - 0.0032 in/in
Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound
BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applic..