Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound

Category Polymer , Thermoset , Polyester, TS , Polyester (Thermoset) - Rigid
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC A50-XHS High Strength Grade Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC A50-XHS is a high strength bulk molding compound. Due to the excellent flow and controlled reactivity, BMC A50-XHS is well suited for injection, transfer or compression molding. Typical applications are circuit breakers, light housings and structural parts.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.79 - 1.85 g/cc
0.0647 - 0.0668 lb/in³
Molded
Linear Mold Shrinkage 0.0015 - 0.0032 cm/cm
0.0015 - 0.0032 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 50
30 - 50
Tensile Strength 57.2 - 71.0 MPa
8300 - 10300 psi
Flexural Strength 124 - 152 MPa
18000 - 22000 psi
Flexural Modulus 11.7 - 13.1 GPa
1700 - 1900 ksi
Compressive Strength 116 - 143 MPa
16800 - 20800 psi
Izod Impact, Notched 5.34 - 6.41 J/cm
10.0 - 12.0 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 V-0
V-0
UL 94 V0/UL 94 5V
Electrical Properties Metric English Comments
Dielectric Strength 14.8 - 16.7 kV/mm
375 - 425 kV/in
short time
Arc Resistance >= 186 sec
>= 186 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F