Polymer Property : Linear Mold Shrinkage = 0.00310 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00310 cm/cm
0.00310 in/in
cure shrinkage
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Ceramic-Filled, Low Expansion, High Lap-Shear Strength & Chemical Resistance, Low Outgassing.