Material Notes:
Ceramic-Filled, Low Expansion, High Lap-Shear Strength & Chemical Resistance, Low Outgassing.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Linear Mold Shrinkage 0.00310 cm/cm
0.00310 in/in
cure shrinkage
Mechanical Properties Metric English Comments
Hardness, Shore D 90.0
90.0
Flexural Strength 93.8 MPa
13600 psi
Shear Strength 13.8 MPa
2000 psi
Thermal Properties Metric English Comments
CTE, linear 25.2 µm/m-°C
14.0 µin/in-°F
Maximum Service Temperature, Air 300 °C
572 °F
Minimum Service Temperature, Air -55.0 °C
-67.0 °F
Electrical Properties Metric English Comments
Volume Resistivity 2.00e+15 ohm-cm
2.00e+15 ohm-cm
Dielectric Constant 4.80

@Frequency 1000 Hz
4.80

@Frequency 1000 Hz
Dielectric Strength 17.7 kV/mm
450 kV/in
Dissipation Factor 0.000700
0.000700
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 93.3 °C
2.00 hour

@Temperature 200 °F
Step 1 of recommended 2 step cure
120 min

@Temperature 177 °C
2.00 hour

@Temperature 350 °F
Step 2 of recommended 2 step cure
480 min

@Temperature 149 °C
8.00 hour

@Temperature 300 °F
Alternate
Pot Life 90.0 min

@Temperature 25.0 °C
90.0 min

@Temperature 77.0 °F
100 g mass
Descriptive Properties Value Comments
Chemical Resistance Excellent
Color Beige
Mix Ratio By Weight 100:5.5
resin:hardener
Viscosity Paste
Users viewing this material also viewed the following: