Physical Properties Metric English Comments
Linear Mold Shrinkage 0.000100 - 0.00260 cm/cm
0.000100 - 0.00260 in/in
Average value: 0.00117 cm/cm Grade Count:3
Overview of materials for Polystyrene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene, Wood Filled". Each property range of values reported is minimum and maximum values of appro..