Physical Properties Metric English Comments
Linear Mold Shrinkage 0.00228 cm/cm
0.00228 in/in
ASTM D955
Plenco 08112 Polyester BMC, Compression Molded
PLENCO 08112 is a renumber of PlasGlas 10112. PLENCO 08112 is a general purpose polyester bulk molding compound that is characterized by adding utility to a number of applications. Because of its co..