Polymer Property : Linear Mold Shrinkage = 0.0017 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ASTM D955
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black
Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products.
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ASTM D955
Plenco 6990 Phenolic, Briquette, Compression Molded
PLENCO 06990 is a glass and mineral filled novolac phenolic molding compound. UL recognized under component file E40654.Information supplied by Plenco.
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
Injection Molding; ISO 2577
Vyncolit X6952 Novolac Phenolic
Glass fiber reinforced phenolic molding compound with superior mechanical properties: very high tensile and flexural strength combined with high elongation at break.USES: Information provided by Vyn..
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ISO 2577
Polyram Polytron P30N11 Polypropylene, 30% Long Fiber Glass
A chemically coupled 30% long fiber glass reinforced natural polypropylene, heat stabilized, for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ISO 2577
Polyram Polytron P30B07 Polypropylene, 30% Long Glass Fibers, UV Stabilized
A chemically coupled 30% long glass fibers reinforced black polypropylene, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
Polyram Polytron P30N01 Homopolymer Polypropylene, Chemically Coupled 30% Long Fiber
A CHEMICALLY COUPLED 30% LONG FIBER GLASS REINFORCED NATURAL POLYPROPYLENE HEAT STABILIZED FOR INJECTION MOLDING APPLICATION.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ASTM D955
Adell DR-16 30% Glass Reinforced Polycarbonate
Linear Mold Shrinkage 0.0017 - 0.0022 cm/cm
0.0017 - 0.0022 in/in
Bulk Molding Compounds BMC T10(14) General Purpose Molding Compound
BMC T10(14) is a general purpose, low shrink molding compound. Due to the excellent flow and controlled reactivity, BMC T10(14) is well suited for injection, transfer or compression molding of intr..
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
Polyram Polytron P30B01 Homopolymer Polypropylene, Chemically Coupled 30% LGF
A chemically coupled 30% LGF reinforced black PP, heat stabilized for high temperature applications such as under the hood automotive parts.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
Polyram Polytron P30B11 Homopolymer Polypropylene, Chemically Coupled 30% LGF
A chemically coupled 30% LGF reinforced black PP, heat stabilized for injection molding applications.Information provided by Polyram Ram On Ind.
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ISO 2577
Polyram Polytron P30N07 Polypropylene, 30% Long Glass Fiber, UV Stabilized
A chemically coupled 30% LGF reinforced natural PP, heat stabilized, UV stabilized for injection molding applications.Information provided by Polyram.
Linear Mold Shrinkage 0.0017 cm/cm
0.0017 in/in
ATM D955
Plenco 50240 PET, Pellet, Injection Molded, Green  (discontinued **)
PLENCO 50240 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for excellent dimensional stability. It is UL listed and available in natural and black..