Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage | 0.00090 cm/cm | 0.00090 in/in | ATM D955 |
Plenco 50130 PET, Pellet, Injection Molded, Natural Color
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |
|||
Linear Mold Shrinkage | 0.00090 cm/cm | 0.00090 in/in | ISO 2577 |
Menzolit Menzolit® BMC 2600 Unsaturated Polyester UP BMC 2600 is a special BMC with reduced electrical properties. The glass content is set to a level that combines good mouldability with good strength and stiffness properties. Because of its improved.. |
|||
Linear Mold Shrinkage | 0.00090 cm/cm | 0.00090 in/in | Borealis Method; anisotropic shrinkage |
Borealis Daplen™ EE158AI Polypropylene TPO Compound Daplen™ EE158AI is a 13% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |
|||
Linear Mold Shrinkage | 0.00090 cm/cm | 0.00090 in/in | ASTM D955 |
Plenco 6015 Phenolic, Briquette, Transfer Molded PLENCO 06015 is a glass and mineral filled phenolic molding compound offering improved mechanical strength, dimensional stability and excellent electrical properties. 06015 is available in black.Inf.. |
|||
Linear Mold Shrinkage | 0.00090 cm/cm | 0.00090 in/in | |
BCC Products BC 7009-2 Epoxy Casting BC 7009-2 is an iron filled, low-cost mass casting system. Recommended for use in casting a minimum of two inches and a maximum of six inches in non-conductive molds. Thicknesses to nine inches in m.. |
|||
Linear Mold Shrinkage | 0.00090 cm/cm | 0.00090 in/in | Cold Part VS Cold Tool; ASTM D955 |
Applied Composites 8007 Polyester SMC Industry Application: ConstructionProduct Application: Water TreatmentDistinct Features: Pigmentable, Low Water Absorption, Weathering Resistant, Good Corrosion Resistance in Waste Water Environment.. |
|||
Linear Mold Shrinkage | 0.00090 cm/cm | 0.00090 in/in | ISO 2577 |
Vyncolit Neopreg Kinel® SK60 L8F Glass Fiber Reinforced Molding Compound Medium flow, epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited f.. |
|||
Linear Mold Shrinkage | 0.00090 cm/cm | 0.00090 in/in | ATM D955 |
Plenco 50130 PET, Pellet, Injection Molded, Black
(discontinued **) PLENCO 50130 is an engineering grade glass reinforced UL flame rated polyethylene terephthalate resin designed for good physical strength. It is UL listed and available in natural and black.Informat.. |