Physical Properties | Metric | English | Comments |
---|---|---|---|
ESCR 100% Igepal® | 16 hour | 16 hour | ASTM D1693 |
LyondellBasell Purell® PE3020D Low Density Polyethylene, Injection Molding, Blow Fill & Seal, Extrusion Blow Molding Purell PE 3020 D is a low density polyethylene with high rigidity, good opticals and good chemical resistance. It is delivered in pellet form. Target markets are small blow molding including packagi.. |