Physical Properties | Metric | English | Comments |
---|---|---|---|
Water Vapor Permeability | 4.60 g mil/ (m2 day) @Temperature 38.0 °C |
0.297 g mil/ (100 in2 day) @Temperature 100 °F |
90% RH; ISO 15106-3 |
Topas Advanced Polymers TOPAS® 9506F-500 Cyclic Olefin Copolymer (COC) TOPAS® 9506F-500 is a high clarity extrusion grade for use in shrink, food and medical packaging as either a discrete layer in multilayer film or in blends with polyethylene. It is designed to del.. |