Polymer Property : Environmental Stress Crack Resistance = 165 hour Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Environmental Stress Crack Resistance >= 165 hour

@Temperature 80.0 °C
>= 165 hour

@Temperature 176 °F
Slow propagation crack resistance, with initial wall stress 4 MPa
Kazanorgsintez PE80B-275 Medium Density Polyethylene Composite
Production Method: Copolymerization of ethylene at low pressure using advanced technology and in presence of complex catalysts on carrier material that allows production of polyethylene with enhanc..
Environmental Stress Crack Resistance >= 165 hour

@Temperature 80.0 °C
>= 165 hour

@Temperature 176 °F
with initial wall stress 4.6 MPa (on pipe samples d110 mm SDR 11)
Kazanorgsintez PE2NT 11-9 High Density Polyethylene Composite
Production Method: Copolymerization of eythylene at low pressure in presence of complex catalysts using gaseous-phase method. Application: Composition is intended to be processed into pressure p..