Physical Properties | Metric | English | Comments |
---|---|---|---|
Base Resin Melt Index | 7.0 g/10 min @Temperature 230 °C |
7.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Lotte Chemical Titan TITANPRO® 6431 Polypropylene homopolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(i) and (c)1.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Melt Index | 7.0 g/10 min @Temperature 230 °C |
7.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Lotte Chemical Titan TITANPRO® EPC40R Polypropylene impact copolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Base Resin Melt Index | 7.0 g/10 min @Temperature 230 °C |
7.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Lotte Chemical Titan TITANPRO® PM430 Polypropylene homopolymer Titanpro® PM430 is designed without any slip agents nor antiblocking agents. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(1)(.. |
|||
Base Resin Melt Index | 7.0 g/10 min @Temperature 230 °C |
7.0 g/10 min @Temperature 446 °F |
ASTM D1238 |
Lotte Chemical Titan TITANPRO® SM461 Polypropylene random copolymer Titanpro® SM461 is formulated with an antiblocking and slip agents package. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i.. |
|||
Base Resin Melt Index | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANZEX® HI1100 High density polyethylene HI1100 is a non UV stabilised high density polyethylene for injection molding. HI1100 meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 21 CFR 177.1520 .. |
|||
Base Resin Melt Index | 7.0 g/10 min | 7.0 g/10 min | ASTM D1238 |
Lotte Chemical Titan TITANLENE® LDC801YY Low density polyethylene resin LDC801YY is a low density polyethylene resin for extrusion coating and is a barefoot grade. LDC801YY meets the U.S. Food and Drug Administration (FDA) criteria for food contact use as specified in 2.. |