Lotte Chemical Titan TITANPRO® SM461 Polypropylene random copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Lotte Chemical Titan Holding Sdn. Bhd. (Former Titan Chemicals)
Trade Name TITANPRO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lotte Chemical Titan TITANPRO® SM461 Polypropylene random copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Titanpro® SM461 is formulated with an antiblocking and slip agents package. The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 177.1520(b). In summary, this resin meets the FDA criteria covering safe use of polyolefin articles and component of articles intended for food contact use. Applications: Heat sealable monolayer film. Heat sealable layer in laminated or co-extruded structures. Quality packaging application.Advantages: Low heat sealing temperature. Good process-ability. Excellent gloss and clarity. Good impact strength at low temperature.Fabrication: Equipment - general film cast machines. Techniques - standard processing. Information provided by Titan ChemicalsCAS# 9010-79-1
Physical Properties Metric English Comments
Base Resin Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Water Absorption 0.020 %
0.020 %
after 24 hrs; ASTM D570
Base Resin Melt Index 7.0 g/10 min

@Temperature 230 °C
7.0 g/10 min

@Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 67
67
ASTM D785A
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 0.932 GPa
135 ksi
ASTM D790B
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °C
158 °F
ASTM D648