Polymer Property : Base Resin Melt Index = 10 g/10 min Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Base Resin Melt Index 10 g/10 min
10 g/10 min
I<sub>21</sub>; ASTM D1238
Lotte Chemical Titan TITANEX® HB0972 High density polyethylene Hexene-1 resin
HF0972 is a pelleted high density polyethylene Hexene-1 resin for blow molding.Applications: Large size shipping containers and drums, household and industrial chemical containers, toiletries and c..