Polymer Property : Base Resin Density = 0.03945 lb/in³ Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Base Resin Density 1.092 g/cc
0.03945 lb/in³
RedEye On Demand Clear PolyJet™ FC720 for Rapid Prototyping
Clear PolyJet Resin (FC720) is a photopolymer resin designed for precise jetting in super fine layers by PolyJet™ Technology, often used in rapid prototyping. Our Clear PolyJet Resin material offer..