Physical Properties | Metric | English | Comments |
---|---|---|---|
Antiblock Level | 1500 ppm | 1500 ppm | SiO<sub>2</sub>; Borealis Method |
Borealis HD621CF Polypropylene HD621CF is a polypropylene homopolymer This grade is suitable for the manufacturing of unoriented films on cast and tubular quench film lines. Applications: food packaging, lamination films, statio.. |
|||
Antiblock Level | 1500 ppm | 1500 ppm | SiO<sub>2</sub>; Borealis Method |
Borealis RD735CF Polypropylene Random Copolymer RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging .. |
|||
Antiblock Level | 1500 ppm | 1500 ppm | |
ExxonMobil LD 143.26 High Clarity Packaging Film Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Antiblock Level | 1500 ppm | 1500 ppm | |
ExxonMobil LDPE LD 136.MN Low Density Polyethylene Resin Product Description: LD 136.MN is a homopolymer film resin with good clarity. The resin is suitable for processing on blown film equipmentAvailability: Latin America, North America and South America.. |
|||
Antiblock Level | 1500 ppm | 1500 ppm | |
ExxonMobil LDPE LD 143.26 Low Density Polyethylene Resin Product Description: LD 143.26 is a homopolymer packaging film resin with excellent clarity and good stiffness. It is suitable for processing in either blown or cast film equipment. In blown film eq.. |
|||
Antiblock Level | 1500 ppm | 1500 ppm | |
ExxonMobil LDPE LD 156HE Low Density Polyethylene Resin Product Description: LD 156 series are LDPE grades, specially designed for lamination films and co-extruded films. They offer good mechanical, stiffness and optical properties, combined with very lo.. |
|||
Antiblock Level | 1500 ppm | 1500 ppm | |
ExxonMobil LDPE LD 361HF Low Density Polyethylene Resin Product Description: LD 361 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Antiblock Level | 1500 ppm | 1500 ppm | |
ExxonMobil LDPE LD 362HE Low Density Polyethylene Resin Product Description: LD 362 series are LEVA LDPE grades, offering good mechanical and sealing properties. Several additive combinations are available according to the required surface properties.Ava.. |
|||
Antiblock Level | 1500 ppm | 1500 ppm | |
ExxonMobil LDPE LD 364HE Low Density Polyethylene Resin Product Description: LD 364HE is an LDPE, offering a good combination of mechanical, optical and sealing properties.Availability: Africa & Middle East and Europe Additive: Antiblock: 1500 ppmSlip: .. |