Physical Properties | Metric | English | Comments |
---|---|---|---|
Slip Level | 2000 ppm | 2000 ppm | EAA; Borealis Method |
Borealis Borclear™ RE936CF Polypropylene Random Copolymer Borclear™ RE936CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: food packaging, lamination films, and stationary fil.. |
|||
Slip Level | 2000 ppm | 2000 ppm | EAA; Borealis Method |
Borealis BorPure™ RD234CF Polypropylene Random Copolymer BorPure™ RD234CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD234CF is recommended for food packaging, stationa.. |
|||
Slip Level | 2000 ppm | 2000 ppm | EAA; Borealis Method |
Borealis Borseal™ RE239CF Polypropylene Copolymer Borseal™ RE239CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films for metallization. Applications: Borseal™ RE239CF is recommended for food packaging, high.. |
|||
Slip Level | 2000 ppm | 2000 ppm | EAA; Borealis Method |
Borealis Borseal™ RE939CF Polypropylene Copolymer Borseal™ RE939CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: Borseal™ RE939CF is designed for: Food packaging,.. |
|||
Slip Level | 2000 ppm | 2000 ppm | EAA; Borealis Method |
Borealis HD234CF Polypropylene HD234CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: HD234CF is recommended for food packaging, lamination films, stationery f.. |
|||
Slip Level | 2000 ppm | 2000 ppm | OAA; Borealis Method |
Borealis HD244CF Polypropylene HD244CF is a homopolymer film resin, suitable for the manufacturing of unoriented film on chill roll process. Applications: food packaging, lamination films, stationery folders, multi layer co-extr.. |
|||
Slip Level | 2000 ppm | 2000 ppm | EAA; Borealis Method |
Borealis RD735CF Polypropylene Random Copolymer RD735CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: RD735CF is recommended for food packaging, textile packaging .. |