Polymer Property : Molecular Weight = 820 g/mol Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Molecular Weight 820 g/mol
820 g/mol
Mw; ETM 300-83
ExxonMobil ESCOREZ™ 5637 Petroleum Hydrocarbon Resin
Light colored aromatic modified, cycloaliphatic hydrocarbon resin. Designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers and metallocene polyolefines. Avail..
Molecular Weight 820 g/mol
820 g/mol
3M Fluorinert™ FC-70 Electronic Liquid
Fluorinert™ Liquid FC-70 a non-conductive, thermally and chemically stable liquid that offers a high boiling point (215 deg C), it is ideal for many electronics single and two phase heat transfer a..