Physical Properties Metric English Comments
Molecular Weight 74.71 g/mol
74.71 g/mol
MV Labs NI800 NiO Nickel(II) oxide
Information provided by MV Laboratories.
Molecular Weight 74.71 g/mol
74.71 g/mol
American Elements Nickel Oxide Nanopowder
General DescriptionNickel Oxide (NiO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Nickel Oxide Particles are typically 10-30 nanometers (nm..