Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 74.71 g/mol | 74.71 g/mol | |
MV Labs NI800 NiO Nickel(II) oxide Information provided by MV Laboratories. |
|||
Molecular Weight | 74.71 g/mol | 74.71 g/mol | |
American Elements Nickel Oxide Nanopowder General DescriptionNickel Oxide (NiO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Nickel Oxide Particles are typically 10-30 nanometers (nm.. |