Physical Properties Metric English Comments
Molecular Weight 720 g/mol
720 g/mol
Mw; ETM 300-83
ExxonMobil ESCOREZ™ 5415 Petroleum Hydrocarbon Resin
Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly..