Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 720 g/mol | 720 g/mol | Mw; ETM 300-83 |
ExxonMobil ESCOREZ™ 5415 Petroleum Hydrocarbon Resin Light colored cycloaliphatic hydrocarbon resin. They are designed to tackify a variety of adhesive polymers including EVA, SIS and SEBS block copolymers, natural rubber, synthetic polyisoprene, poly.. |