Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 65000 g/mol | 65000 g/mol | M<sub>w</sub> |
Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed Product Description: Epolene C-26 is a maleic anhydride grafted polyethylene coupling agent for polyethylene (PE) composites. The polar functionality and molecular weight are optimized to provide ba.. |