Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed

Category Polymer , Thermoplastic , Polyethylene (PE)
Manufacturer Westlake Chemical Corporation
Trade Name Epolene®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Westlake Epolene® C-26 Coating Grade - Highly Branched Medium Molecular Weight Polyethylene Polymer, Maleation Processed.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Epolene C-26 is a maleic anhydride grafted polyethylene coupling agent for polyethylene (PE) composites. The polar functionality and molecular weight are optimized to provide balanced attraction between PE and reinforcements / fillers like glass, wood, minerals, and metals. Epolene C-26 Polymers are products of Westlake Chemical Corporation and are protected under one or more of the following U.S. patents: 5,955,547 and 6,046,279; and their foreign equivalents. Key Attributes:Balances attraction between polar fillers/reinforcements and non polar polymersCoupling agent for PE compositesMaleic anhydride grafted polyethylene(PE)Application/Uses:Automotive OEM Building and Construction Rubber and Plastic Modification
Physical Properties Metric English Comments
Specific Gravity 0.910 - 0.920 g/cc
0.910 - 0.920 g/cc
Brookfield Viscosity 8.0 cP

@Load 0.00000220 kg,
Temperature 190 °C
8.0 cP

@Load 0.00000475 lb,
Temperature 374 °F
Molecular Weight 65000 g/mol
65000 g/mol
M<sub>w</sub>
Melt Flow 2.0 - 10 g/10 min
2.0 - 10 g/10 min
PTM-008
Thermal Properties Metric English Comments
Ring & Ball Softening Point 122 °C
252 °F
DSC Tm; ASTM E28
Optical Properties Metric English Comments
Gardner Color Number <= 11
<= 11
VCC-099
Chemical Properties Metric English Comments
Total Acid Number 8.0
8.0
ASTM D1386
Descriptive Properties Value Comments
Penetration Hardness <1 dmm
ASTM D5, Needle under 100-g load for 5s @ 25 deg C, tenths of mm