Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 509.69 g/mol | 509.69 g/mol | |
M Chemical GUARD DOGâ„¢ UV1164 Light Absorber, Triazene Derivative GUARD DOGâ„¢ UV1164 light stabilizer is a derivative of Triazine that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout t.. |