Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

M Chemical GUARD DOGâ„¢ UV1164 Light Absorber, Triazene Derivative

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer M Chemical Company, Inc.
Trade Name GUARD DOG™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF M Chemical GUARD DOGâ„¢ UV1164 Light Absorber, Triazene Derivative.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
GUARD DOG™ UV1164 light stabilizer is a derivative of Triazine that has an exceptionally strong and broad-range of UV absorption properties (UV A 315 -400 nm and UV B 290 - 314 nm) throughout the UV spectrum. It is a highly efficient UV absorber and is recommended for thermoset plastics and coatings that function as ultraviolet screens for photosensitive substrates.Applications: It is mainly used in polycarbonate, polystyrene, acrylate, olefin, hydrocarbon, etc. It has good compatibility and low volatility and can be used in combination with other UV absorbers. It is used in PE or PP film, tape, Sheet and other resin systems such as Polyamides, PET, ASA, PETG, PMMA, PBT and PC (cap stock and general purpose). Performance Benefits:Strong and broad UV absorption with minimal color contribution. High thermal stability (10% wt. loss at 347°C)Minimal interaction with metals and has high permanence (low volatility and high light stability).Excellent compatibility with engineering polymers, polyolefins and other stabilizer chemistries.Typical Properties:Light yellow powderSolubility (g/100g @ 25°C): Butanol 3.0, BA and MEK 17.0, Xylene 25.0, 1methoxy-2- Propanol Acetate 11.0Max, nm: 293 & 342
Physical Properties Metric English Comments
Specific Gravity 1.15 g/cc

@Temperature 25.0 °C
1.15 g/cc

@Temperature 77.0 °F
Molecular Weight 509.69 g/mol
509.69 g/mol
Thermal Properties Metric English Comments
Melting Point 88.0 - 91.0 °C
190 - 196 °F
Descriptive Properties Value Comments
CAS Number 2725-22-6
Molecular Formula C33H39N3O2
Name 2-[4, 6-Bis (2, 4-dimethylphenyl)-1, 3,5-triazin-2-yl)]-5-(octyloxy) phenol
Recommended Dosage 0.05 - 1.0 wt%