Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 447.6 g/mol | 447.6 g/mol | |
Hong Kun Group UV 234 UV Absorber UV 234 is a high molecular weight ultraviolet light absorber (UVA) of the hydroxyl phenyl benzotriazole class, imparting outstanding light stability to polymers usually processed at high temperature.. |