Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 447.58 g/mol | 447.58 g/mol | |
M Chemical GUARD DOG™ UV234 Light Absorber, Benzotriazole Derivative GUARD DOG™ UV234 UV absorber is a low volatile benzotriazole based UV absorber which is highly effective in polymers that are processed at high temperature (decomposition temperature > 350°C.. |