Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 418 g/mol | 418 g/mol | |
BASF Palatinol® N Diisononyl Phthalate Formula: C28H42O4Description: Palatinol® N is an excellent primary plasticizer for plasticized vinyl articles. Its compatibility with vinyl is good even in high concentrations. Palatinol N in vinyl.. |