Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 360000 g/mol | 360000 g/mol | Mv |
Lucite International Colacryl ® TS2082 Acrylic Resin Colacryl® TS2082 is a solid bead resin with low residual peroxide content, specially designed for use in a variety of industrial and dental applications. In dental applications the product is typ.. |