Lucite International Colacryl ® TS2082 Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA)
Manufacturer Lucite International
Trade Name Colacryl ®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Lucite International Colacryl ® TS2082 Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Colacryl® TS2082 is a solid bead resin with low residual peroxide content, specially designed for use in a variety of industrial and dental applications. In dental applications the product is typically used to modify the handling characteristics of pourable systems.Typical industrial uses include viscosity modification of reactive composites and thickening of cyanoacrylate adhesives, due to the absence of Lewis bases. It may also be used in the formulation of porous polymer mold compositions.Information provided by Lucite International
Physical Properties Metric English Comments
Viscosity Measurement 1.8
1.8
reduced, 1% solution in chloroform; Ubbeholde OB viscometer
Molecular Weight 130000 g/mol
130000 g/mol
Mn
360000 g/mol
360000 g/mol
Mv
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 105 °C
221 °F
Processing Properties Metric English Comments
Moisture Content 0.50 %
0.50 %
Descriptive Properties Value Comments
Benzoyl Peroxide Content (%) <0.1