Physical Properties | Metric | English | Comments |
---|---|---|---|
Molecular Weight | 325.82 g/mol | 325.82 g/mol | |
MV Labs CS300 Cs2CO3 Cesium carbonate Information provided by MV Laboratories. |
|||
Molecular Weight | 325.82 g/mol | 325.82 g/mol | |
American Elements Lanthanum Oxide Nanopowder General DescriptionLanthanum Oxide (LaO) Nanoparticles, nanodots or Nanopowder are white spherical high surface area metal particles. Nanoscale Lanthanum Oxide Particles are typically 10-30 nanomete.. |